Categories
Price: | Negotiable/Piece |
---|---|
Min Order: | 1 /Piece |
Prod Model: | GLC-EPTANK 364 |
---|---|
Markets: | North America,South America,Eastern Europe,Southeast Asia,Africa,Oceania,Mid East,Eastern Asia,Western Europe |
Use: | Appliance Paint |
Appearance: | Liquid |
Level: | Finish Coat |
Substrate: | Steel |
Method: | Spray, Brush or Roller |
GREEN LEAF CHEMICAL LIMITED | |||||||
GREEN LEAF Handbook of industrial protective coatings |
Phenolic epoxy paint tank EPTANK 364 white yellow |
||||||
Application | Thin film coatings for storage tanks can be loaded with wide range of products, including the loading of gasoline , alcohol mixture, tank containing 65 degree centigrade ~ 100 degree centigrade hot water and container wall. | ||||||
Products Introduction | Two cans, phenolic epoxy tank coating. | ||||||
Product data | Solid volume | 50% | |||||
Dry film thickness | The equivalent of 125 microns to 250 microns wet film thickness | ||||||
Theoretical spreading rate | 2.7m2/kg, according to required volume solids and dry film thickness of 125 micron meter. | ||||||
Practical Coverage | Allow appropriate loss | ||||||
Works described in detail | Mixing ratio | A: B = 4:1 (weight ratio) | |||||
Construction method | |||||||
Airless spray |
Recommended use: Tip range 0.53 ~ 0.68mm(21~27) Total fluid pressure of vent no less than17.6MPa (176kg / cm2) |
||||||
Brush or roller | Applies only to a small area. Need to repeat the coating, in order to achieve the required dry film thickness. | ||||||
Conventional spray | Not recommended | ||||||
Thinner | Under normal do not need to, if necessary, with the BW 103 | ||||||
Reaction induction time | 15min (at 10 degree centigrade ~ 35 degree centigrade conditions) | ||||||
Use of | 10 degree centigrade ~ 35 degree centigrade, 1 hour (induct rising from the reaction) | ||||||
Drying time | |||||||
Substrate temperature | Surface dry (h) | Completely dry (h) | Repeat brushing interval | ||||
The shortest | The longest | ||||||
5 degree centigrade 23 degree centigrade 35 degree centigrade |
6 3 1 |
12 3 1 |
24h 24h 24h |
14days 14days 14days |
|||
Storage and management | Storage | Store in a cool and dry environment. | |||||
Flashpoint | Greater than 20 degree centigrade (composition or mixture) | ||||||
Packing |
A: 20 kg in the 20 liter container B: 5 kg in 10 liter containers |
||||||
Proportion | 1.49 kg/ liter | ||||||
Technical requirements and surface treatment |
Contact the Company on the construction details of cabin interior coatings By coating the surface must be clean, dry and free from contamination, according to SSPC-SP1 solvent cleaning to remove surface oil, remove the residues and planish sharp edges , sandblasted to Sa2.5 (Sweden Standard SIS055900) The coating must be completed before the steel re-oxidation coating, if oxidation has occurred, to be fully re-oxidized part of the sand to the required standards. Heat sink If a little rusty on hot water tank wall, to be sandblasted in accordance to the Swedish standard SIS055900 Sa1, and rinse, dry and then sand to Sa2.5 (Swedish standard SIS055900). |
||||||
Restrictions | This product is below 5 degree centigrade can not be fully cured, for the sake of the appropriate curing effect, plate temperature should be above 10 degree centigrade, and at least more than 3 degree centigrade above the dew point, relative humidity shall not exceed 80%. | ||||||
Safety measures | See“Summary of Paint" |