| Supplier: | Hebei Ruide Group Sanxing Rubber & Plastic Co., Ltd |
|---|---|
| Price: | US $ 6.5/Meter |
| Min Order: | 5000/Meter |
| Quantity:: | |
| Trade Terms: | FOB |
|
|
| Prod Model: | SX3017 |
|---|---|
| Markets: | North America,South America,Eastern Europe,Southeast Asia,Africa,Oceania,Mid East,Eastern Asia,Western Europe |
| ID=50 Mm: | Od=52 Mm |
| Thickness=1 Mm~20 Mm: | Color: Grey or Customized |
| Material: | TPU |
| key word | TPU straight corrugated hose |
| Material | high quality import silicone/EPDM/PVC/TPU/TPV/TPE/PE |
| Size | Custom Design will be acceptable, wide size range can be accept |
| Color | blue,grey or customized |
| Adhesive strength, k N/m | ≥1.5 |
| Brittle temperature ( -50 °C × 4h ) | No craking |
| Ozone resistance ,( 50 ± 5 ) mPa ,( 70 ± 2 ) h × ( 40 ± 2 )°C | No cracks and visible change |
| Air aging ( 110 °C ×72h ) | No cracks and visible change, hot air aging test after bending, radius should be less than 80 mm. |
| Out-of roundness | The roundness of the telescopic pipe is not greater than 5%, when the test after the bend radius (or repeated bending after 5 times) out of roundness is not greater than 10%. |
| Toroidal pressure resistant | When the pipe deformation 2mm in diameter, pressure should not be less than 120N. |
| Bending radius | Should be less than 60 mm (bending center to the expansion pipe); bending radius should be less than 80 mm after the hot air aging. |
| Fire resistance |
Meet the GB 8410-2006 |