Categories
| Supplier: | Hangzhou Ualloy Material Co., Ltd. |
|---|---|
| Price: | US $ 18-18.2Kilogram |
| Min Order: | 20Kilograms |
| Quantity:: | |
| Trade Terms: | FOB,CFR,CIF |
|
|
| Prod Model: | 4J29 |
|---|---|
| Markets: | North America,South America,Eastern Europe,Southeast Asia,Africa,Oceania,Mid East,Eastern Asia,Western Europe |
| Condition: | Bright |
| Density: | 8.17 g/cm3 |
| Thermal Expansion Coefficient (20~300oc): | 5.0*10-6 /Oc |
| Thermal Expansion Coefficient (20~450oc: | 5.2*10-6 /Oc |
| Curie Point: | 430oc |
| Volume Resistivity (20oc): | 46ohm.Cm |
| Thermal Conductivity: | 20.3W/M. Oc |
| Hardness(Temper Rolled): | 230 Hv |
| Packing Detail: | Coil (Plastic Spool) + Compressed Ply-Wooden Case |
| Certification: | ISO9001 |
| Product Type: | Wire |
| Carbon Content: | Low Carbon |
| Material: | Nicofe |
Mn | Ni | Co | C | Si | P | S | Fe |
0.25 | 29.1 | 17.3 | 0.015 | 0.12 | 0.006 | 0.005 | Bal |
Density | 8.17 g/cm3 |
Thermal Expansion Coefficient (20~300ºC) | 5.0*10-6 /ºC |
Thermal Expansion Coefficient (20~450ºC) | 5.2*10-6 /ºC |
Curie Point | 430ºC |
Volume Resistivity (20ºC) | 46μΩ.cm |
Thermal Conductivity | 20.3W/m. ºC |
Temper rolled | As annealed | |
| Yield Strength | 695 Mpa | 315 Mpa |
| Tensile Strength | 780 Mpa | 520 Mpa |
| Elongation | 5% | 24% |
| Hardness | 230 HV | 48 HV |