Types | HR-RT5101 | HR-RT5110 | HR-RT5111 | |
Performance | Light colour.Excellent Green Tack,lowers Mooney viscosity of compound.has limited influence on vulcanization time and physical properties after vulcanization. Lowers hardness and modulus of compound after vulcanization.improves extension and chipping resistance performances. Help fillers distritute evenly,Avoid adhesion to compounding equipment | |||
Application | Recommended Application: Tire Rubber Compounding Other Applications: Compounding of other rubber products.like shoe sole.heel.flooring.rubber belts.rubber tube.Light-colour rubber,Pressure Sensitive adhesive |
Properties\Types | HR-RT5101 | HR-RT5110 | HR-RT5111 | TEST METHOD |
Class | C5 | C5/C9 | C9 | -- |
Appearance | Granule | Granule | Granule | Eyeballing |
Softening Point (oC) | 95-105 | 95-105 | 95-105 | ASTM E 28 |
Color No.(Ga#) | 5 | 10 | 11 | ASTM D 1544 |
Acid Value ( mgKOH/g ) | ≤1.0 | ≤0.5 | ≤1.0 | ASTM D 974 |
Bromine Value (gBr/100g) | 20-100 | 50-110 | 50-110 | ASTM D 1959 |
Melt Viscosity (BRF,@200oC ) | ≤260 | -- | -- | ASTM D 3236 |
Flash Point (oC) | Test if need | GB261 / GB3536 |