Categories
Price: | US $ 1000/Ton |
---|---|
Trade Terms: | FOB,CFR,CIF |
Min Order: | 25/Ton |
Pay Type: | L/C,T/T |
Packaging Detail: | 25kgs bag,21tons/20'fcl |
Delivery Detail: | 15 days |
Properties | Unit | Test method | Value |
Melt Flow Rate | |||
Melt flow rate(230°C/2.16KG) | g/10min | ISO 1133 | 12 |
Mechnical Properties | |||
Tensile modulus of elasticity(v=1mm/min) | Mpa | ISO 527-2 | 1550 |
Tensile yield at stress(v=50mm/min) | Mpa | ISO 527-2 | 35 |
Tensile yield at strain (v=50mm/min) | % | ISO 527-2 | 8 |
Tensile strain at break (v=50mm/min) | % | ISO 527-2 | >50 |
Charpy impact strength unnotched(+23°C) | kJ/m2 | ISO 179/1eU | 110 |
Charpy impact strength notched(+23°C) | kJ/m2 | ISO 179/1eA | 3.0 |
Izod Impact strength notenched(+23°C) | kJ/m2 | ISO 180/1A | 3 |
Ball indentation hardness(H 358/30) | Mpa | ISO 2039-1 | 78 |
Tests | Value | Unit |
Melt Flow Rate | 45 | g/10min |
Density | 0.90 | G/cm3 |
Elongation Stress | 10 | % |
Flexural modulus | 14 | Mpa |
Rockwell hardness | 95 | R scale |
IZOD impact strength | 6.5 | kg.cm/cm |
Vicat softening point | 152 | °C |
Heat distortion temperature | 125 | °C |
Tests | Value | Unit | Method |
Melt Flow Rate (MFR) | 0.45 | g/10min | GB 3682 |
Density | 0.91 | g/cm3 | ASTM D-1505 |
Tensile Strength at Yield | 24 | Mpa | GB 1040 |
Elongation at Break | 750 | % | GB 1040 |
Rockwellhardness | 85 | J/M | GB 9342 |
Izod impact strength | 65 | J/M | ASTM D-256 |
Prod Model: | virgin/recycled/ repro |
---|---|
Markets: | North America,South America,Eastern Europe,Southeast Asia,Africa,Oceania,Mid East,Eastern Asia,Western Europe |
Resin P P: | White |