Categories
Price: | US $ 1.5-2.5kilogram |
---|---|
Trade Terms: | FOB |
Min Order: | 5/Ton |
Pay Type: | L/C,T/T |
Product Name: Aluminum Alloy Zincate Process HN-3000
Bath Composition and Working condition:
HN-3000: 550~600ml/L
Temperature: 16~30°c
Time: 20~120 seconds
Application and Advantages:
1. Alloy layer of zinc, copper, iron and nickel.
2. Good adhesion though in aluminum alloy of low purity.
3. After zinc settling, chemical nickel or bright nickel can be plated directly.
4. Using HN-3000C and HN-3000B to supplement metal and alkali that makes the solution stable and easy to control. Using HN-3000 alone for supplement is OK.
5. Especially suitable for plating aluminum alloy wheels.
Company Information:
Prod Model: | HN-3000 |
---|---|
Markets: | North America,South America,Eastern Europe,Southeast Asia,Africa,Oceania,Mid East,Eastern Asia,Western Europe |
Classification: | Chemical Additives |
Appearance: | Liquid |
Color: | Green |
Efficacy: | Electroplating |