Shanghai Sepuna Chemical Technology Co., Ltd. >> Flame-Retardant Epoxy Potting Adhesive Sealant

Flame-Retardant Epoxy Potting Adhesive Sealant

Flame-Retardant Epoxy Potting Adhesive Sealant
Supplier: Shanghai Sepuna Chemical Technology Co., Ltd.
Price: US $ 3.55-3.85/Piece
Min Order: 2000/Piece
Quantity::
Trade Terms: FOB,CFR,EXW
contact supplier

Product Specifications

Prod Model: E4212
Markets: North America,South America,Eastern Europe,Southeast Asia,Africa,Oceania,Mid East,Eastern Asia,Western Europe
Brand Name: Punade
Model Number: E4212
Propetry: Waterproof, Moisture/Temperature Resistance
Certificate: CE, SGS, ISO9001:2000, MSDS, UL, RoHS
MOQ: 500-2000 PCS
Samples: Free Sample
Delivery Time: Fastest Delivery(5-7days)
Shipping: by Express(FedEx, UPS, DHL, TNT), or by Sea
Manufacturer: R&D Manufacturer, Factory, China Supplier
Clients: Lonking, Jabil, Dongfeng Group, Cummins, Volvo
Classification: Room Curing
Application: Packing
Material: Polyurethane
Characteristic: Waterproof
Morphology: Solvent-Free
Color: Black/White

Product Description

Flame-retardant two component epoxy potting adhesive sealant Features After curing flame retardant UL 94 V-0 and other properties are same as 6102 Use For potting of flame retardant for small and medium - sized and closing of the circuit board, such as capacitor coating, solid state relay potting, etc Operation 1. Stirring A component evenly before using it. 2. Weighed in a 5: 1 ratio A, B two components, stir well stay with after vacuum deaeration to use within 60 minutes run out. 3. Good potting devices, if necessary, continue to pumping vacuum, help to increase the electrical performance of the device. 4. Curing conditions: 25° C for 24hrs at room temperature; Or let stand for surface bubbles after heating 65 ° C× 0.5hr. 5. Note: Adhesive start the reaction after adhesive preparation, accompanied by heat release. With the greater amount of glue, the greater the heat release, the shorter operating time, required in a shorter period of time you are finished using 6. The above tests are measured under 100 g with adhesive Package & Storage Package ? ? ? ? ? ? ? ? ? ? ? ? ? ? ?Storage Part A: 25kg/bucket ? ? ? ? ? ? Seal and Avoid light and light 5kg/bucket ? ? ? ? ? ? ? ? ? ? ? ? ?Temperature≤ 25° C, humidity≤ 50%RH Part B: 5kg/pot ? ? ? ? ? ? ? ? ? ?Shelf life: Part A 6 months, Part B 6 months 1kg/pot Out standing customer care services at any time, 24 Hour Help Support on line or or call +86-400-882-1323
Test Item 4202 4205 4208 4215 4212
Properties 
before 
curing
 
Appearance  liquid cement A Black ropy fluid Black ropy fluid  Transparent fluid  Black ropy fluid Black ropy fluid 
liquid cement B  Brown liquid  Brown liquid Transparent fluid  Transparent fluid Brown liquid 
Density,g/cm3
25 °C
liquid cement A 1.85~1.95 1.85~1.95 1.05~1.15 1.85~1.95 1.85~1.95
liquid cement B 1.10~1.13 1.12~1.15 0.94~0.96 1.10~1.13 1.10~1.13
Mixed 1.50~1.60 1.50~1.60 0.99~1.01 1.50~1.60 1.50~1.60
Viscosity,cps
25 °C
liquid cement A 12000~18000 12000~18000 1500~1800 12000~18000 12000~18000
liquid cement B 100~300 500~800 300~500 40~120 40~120
Mixed 900~1300 1500~2000 600~900 900~1300 900~1300
Mixture/mass ratio, weight 5:1 5:1 2:1 7:1 5:1
Usable time , hr ,25 °C ,100g 1 1 0.5 1.5 1
Preliminary curing time hr,25 °C 4~6  6~8  3-4 2~3(Under 80 °C ) 6~8
Completely cure time,hr, 25 °C 24 24 24 24 24
 
Properties 
after 
curing
Hardness ,Shore-D >85 >85 >85 80-85 >85
    Volume resistance,Ω.cm,25 °C 2.8×1015 1.5×1015 1.2×1015 1.2×1014 1.2×1015
Breakdown Voltage,kV/mm,25 °C >30 >30 >30 >25 >30
Dielectric constant ,1.2MHz,25 °C 3.1±0.1 3.2±0.1 3.3±0.1 3.1±0.1 3.3±0.1
dielectric loss tangent,1.2MHz <0.01 <0.01 <0.01 <0.02 <0.01
curing shrinkage rate,% <2 <2 <2 <0.8 <2
Tensile-shear strength,Fe-Fe,MPa >10 >10 >10 >10 >10
Operating temperature range, °C -40~100 -40~100 -40~100 -40~180 -40~100
Flammability class UL 94 - V-2 - V-2 V-0

Founded in DEC. 2003, SEPUNA has been engaged in researching, manufacturing and marketing automobile sealant and adhesive for 9 years.

Since the foundation, SEPUNA Chemical has been focusing on adhesive's researching and application. Then in 2005, We acquired PUNADE technology which is from Switzerland.

Within 9 years, SEPUNA mainly develops Silicone, Polyurethane and Epoxy resin adhesives. And in the future, we will enlarge our line to Unsaturated, Natural and Acrylic Resin adhesive.

After 9 years' improvement, by the keep researching and innovation, SEPUNA is already a mature adhesive supplier with the core competitiveness.

Send your message to this manufacturer

  • Inquiry about Flame-Retardant Epoxy Potting Adhesive Sealant

Other Products From This Manufacturer